The furnace body of a medium frequency furnace consists of four main parts: furnace shell, induction coil, furnace lining and furnace tilting device. The furnace shell is made of non-magnetic materials, and the induction coil is wound into a spiral cylinder by rectangular hollow copper tubes, with cooling water flowing through the tubes during smelting. The lead-out copper bar of the coil is connected to the water-cooled cable, the furnace lining is closely attached to the induction coil, and the tilting of the furnace body is directly driven by the furnace tilting reduction gearbox. Due to process or operation reasons, the copper bar is sometimes burned through by molten iron, which causes hot furnace shutdown.
During the operation of a medium frequency furnace in a company, the copper bar burn-through fault occurred many times, and there are two main causes: first, careless operation during tilting pouring or an overly short furnace mouth causes splashed molten iron to adhere to the copper bar and burn it through; second, after the furnace lining is burned through, overflowing molten iron causes the copper bar to burn through.
Copper bar burn-through causes cooling water overflow, so the furnace must be shut down immediately for repair. Since the copper bar is installed inside the furnace shell, welding repair is inconvenient, and it needs to be disassembled and taken out for repair. The traditional copper bar repair process is: Tilting furnace to discharge molten iron → Shutdown → Cooling → Removing furnace lining → Taking out copper bar → Welding repair of copper bar → Installing copper bar → Building new furnace lining → Furnace drying → Furnace startup.
This repair method wastes at least one furnace lining, three shifts of man-hours and a large amount of electric power.
The following introduces a bonding method for repairing copper bars, which is more energy-saving and time-saving.
For copper bar burn-through caused by the first reason, you can temporarily shut down the furnace, cut 1~2 mm thick copper sheets into small pieces, whose area should be slightly larger than the area of the burn-through crack on the copper bar. Then remove the residues at the burn-through site of the copper bar with a saw blade or an electric hand grinder, polish it clean with sandpaper, quickly mix the shaped epoxy resin with curing agent, and bond the trimmed copper sheet to the crack of the copper bar. After a few minutes, the epoxy resin solidifies and can form high bonding strength for the copper bar, and the furnace can be restarted at this point.
For copper bar burn-through caused by the second reason, the repair process is as follows: Tilting furnace to discharge molten iron → Shutdown → Furnace lining repair → Copper bar bonding repair → Furnace startup. Compared with traditional welding repair, this repair process also saves one furnace lining, a lot of man-hours and electric power for furnace drying.